2023-10-19
Partial plating
In our company's salt spray test, the salt spray resistance of SUS316 electroplating can reach 600H, the salt spray resistance of magnet electroplating can reach 240H, the strong acid sweat resistance of brass electroplating can reach 240H, and the electrolysis resistance of brass electroplating can reach 120Min. Far exceeding industry standards.
Magnet surface treatment
The magnet surface treatment in the laboratory can achieve: salt spray resistance test (NSS) ≥ 240H, RCA test (175g) ≥ 500t, adhesion test ≥ 50t, friction coating hardness pencil measurement ≥ 5H, acid sweat resistance test ≥ 168H, Unconventional temperature and humidity cycle test ≥ 21 Days.